ABS plastik se yon kalite materyèl "difisil, difisil ak rijid" ak matyè premyè fasil disponib, bon pèfòmans konplè, pri ki ba ak aplikasyon lajè. Plastik ABS te lajman itilize nan machin, elektrik, twal, otomobil, avyon, bato ak lòt endistri manifakti ak endistri chimik.
Voye rechèch
Dekri teren
Karakteristik teknik

Entwodiksyon nan karakteristik ak varyete ABS plastik matyè premyè



ABS plastik matyè premyè (acrylonitrile-butadiene-styrene) non angle: Acrylonitrile butadiene styrene

Espesifik gravite: 1.05 g/cm3

Kontraksyon bòdi: 0.4-0.7 pousan

Tanperati bòdi: 200-240 degre

Kondisyon siye: 80-90 degre pou 2 èdtan

Pwopriyete materyèl plastik ABS



1. Bon pèfòmans konplè, fòs enpak segondè, estabilite chimik ak bon pwopriyete elektrik.

2. Li gen bon fizyon ak 372 plexiglass, epi li ka fèt an pati plastik de koulè, ak sifas la ka chrome-plake ak espre-pentire.

3. Gen gwo rezistans enpak, segondè rezistans chalè, rezistan flanm dife, ranfòse, transparan ak lòt klas.

4. Fluidité a se yon ti kras pi mal pase HIPS, pi bon pase PMMA, PC, elatriye, ak fleksibilite a se yon bon bagay. Li se apwopriye pou fè pati jeneral mekanik, mete-diminye ak mete ki reziste pati, pati transmisyon ak pati telekominikasyon.


ABS plastik materyèl bwit bòdi pwopriyete


1. Materyèl amorphe, ak likidite mwayen ak absòpsyon imidite segondè, yo dwe konplètman cheche. Pati plastik ki gen sifas briyan dwe prechofe epi seche nan 80-90 degre pou 3 èdtan pou yon tan long.

2. Li rekòmande pou pran tanperati materyèl segondè ak tanperati mwazi segondè, men li fasil pou dekonpoze si tanperati materyèl la twò wo (tanperati dekonpozisyon an se > 270 degre). Pou pati tèrmoplastik, tanperati mwazi an ta dwe 60-80 degre.

3. Pou rezoud streak dlo a, li nesesè amelyore likidite materyèl la, adopte metòd tankou tanperati materyèl segondè, tanperati mwazi segondè, oswa chanje nivo dlo a.

4. Si materyèl ki reziste chalè oswa rezistan flanm dife yo fòme, pwodwi dekonpozisyon plastik yo ap rete sou sifas mwazi an apre 3-7 jou pwodiksyon an, ki pral lakòz sifas mwazi an klere. Mwazi a bezwen netwaye nan tan, ak sifas mwazi an bezwen ogmante pozisyon tiyo echapman an.


Entwodiksyon de varyete plastik ABS materyèl bwit


Taiwan Chimik AG15A1 AG15A0 AG15AS(BK) AG10AP AG10NP AG12A0 AG15E1 AG15A2 ANC120 AE8000 AT5500


Bèljik BASF GP-22 GP-35


Changsu Nouvo Materyèl CF-610A CF-610T


Changzhou Hanbang FR-800 FR-800A


BASF 2802-TR GP-35 13010 2812TR 928SG3 GP-22 HH-112 HI-12


Bayer, Almay 150G22-901510


LANXESS NP2H-AT P2H-AT P2MC


Guangzhou LG AF-312B AF-312C AF-342(BK) HI-121H HF-380


Guangzhou Blonde FW-620HT (BK) 612 GAR-011 GF20(NC) HF-606 HF-630 HF630 NC


Kore LG HI-100 HI-121H AF-312T AF-303S AF-305L AF-312B AF-312C TR-530F AF-368-17127 HF-380 GP{-2100 GP-2200 GP-2305 TR-557 TR-557I TR -558A TR-558AI XG-570 XR-401 XR-404N XR-407E XR-409H


Kore di Kumho 720V 750N 750SW HAG5210FR ER875 HAG5220FR HAG5230FR HAG7210 HAG7220 HAG7230 HAM-8560 HFA452 SF-0505EA(BK)


Kore di Samsung First Knitting VH-0815


Hyosung BASF GP-22


Hansamsung premye tise lenn mouton AS-0150 GR-4020 HF-0660I VH-0815T QHF-0140 HF-0680U HG-0760GP SD-0150 SD-0150W SF-0505(BK) SF-0505EA(BK) SF-0509T CT- 0520 VH{{13} } VH-0810T VE-0860 UT-0510T UT-0800 VH-0800E VH-0815-W92747


Basic Innovation Plastics (USA) BDT6500-1000 MG37EP-NA1000 X17-1000 BDT5510-1000 FR15U-NA1000 VW300-1000

FR15-NA1000 MG29-NA1000 FR15U X15-1000


Toray Malezi 700 100 920


Dow 3904


Azòt likid Ameriken AF3009 AF3029U AFFRUV STATLOY-AFR AL-4010 AL4020 BK8-115


INEOS M202AS


Ningbo LG HI-121H HT-550 FR-500(YX)


Ningbo Taihua AG15A1 AG15E1 AG15AI


Japan NIPPON A&L ANG-10 BK901 ANG-15 BK901 ANG-20 BK901 ANG-20 GY ANG-5 WH GA-110G10 PH646 GA{{11 }} BK ST-400


Japon TECHNO F{{0}}V0-BK F5330G20-V{0 F{5330-V0 F7850- V0


Japon UMG 3001M GF10 GF20 VD210 ESA20 3001M (BK) FA820C1 EX19C-450 (BK) FA-830CA KJB{-11001 MG-510A TJ3L TM{{ 13}} TM-21 TM-30 TW17 (BK) V6100A 9180 (GY) U4800 VG4 -11001 U400B


Daicel 462M 660 LMW48


Nippon Denki TP-RX-301 TP-UR10G TP-URX AF-5350 APT-3010 APT-AL81 KX-314 TH-9S TX-100 S AT-07 M1-5150X{-301 SM050 TP-SX-301 TP-URX- 50 TH-21 TP-801 AC{ {22}} CL CL-301 CU-301 GR-2000 T180 UT30B


Toray 100 100G-10 100G20 100G-30 700 824V 920 (BK) ASG-40 AX05 855VG10 700-BK 834V 855V 900 920 ASG30 GDT-03 (NC) VX10G15-BK 844V (BK) TP90 VX1


Mitsubishi Jeni Japonè VPG120


Panasonic Corporation MBW900T


Dow 720GS


Maru Petrochemical TW{{0}}V0 TW-03V0

Asahi Kasei SM050 SM05N SX-200 IM15 VA507 (V0) AT900 BK


Lank Japon T-100 TI-300 TI-500A


Sumitomo KU-600R-1 KU650 KU650R


Sumitomo Northrop Grumman 600R



extrudée abs plastik pwofil foto:

Extruded abs  profile

Extruded abs plastic profile



Baj popilè: extruded abs plastik pwofil, Lachin, Swèd, manifaktirè, faktori, Customized, achte, te fè nan peyi Lachin